Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 5.0 - 10000 ohm | 5.0 - 10000 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Surface Resistance | 5.0 - 8.0 ohm | 5.0 - 8.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC LNP* STAT-KON* D-FR is a compound based on Polycarbonate resin containing Carbon. Added features of this grade include: Flame Retardant, Electrically Conductive. |
|||
Surface Resistance | 5.0 - 8.0 ohm | 5.0 - 8.0 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon TE002 LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Surface Resistance | 5.0 - 8.0 ohm | 5.0 - 8.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON TE002 PU LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Surface Resistance | 5.0 ohm | 5.0 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon DX02731C PC LNP STAT-KON* DX02731C is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |