Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 10000 ohm @Thickness 0.400 mm |
<= 10000 ohm @Thickness 0.0157 in |
ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PE 1313
(discontinued **) PRE-ELEC PE 1313 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 13.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® 12-032
(discontinued **) PRE-ELEC 12-032 is a conductive thermoplastic compound based on a polyacetal copolymer with 20% carbon fiber. PRE-ELEC 12-032 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1105-7852 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1105-7995 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1105-8354 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1105-8355 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1200-8493 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 19-7278 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 50-7289/V2 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 50-7856/FR/BK Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/BK Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Surface Resistance | 10000 ohm | 10000 ohm | ASTM D257 |
Techmer ES Electrablend® PC SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr.. |
|||
Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics ULTEM JD7101 PEI (Asia Pacific) |
|||
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX03550 PC (Asia Pacific) LNP STAT-KON* DX03550 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 10000 - 1.00e+6 ohm | 10000 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy .. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | ASTM D257 |
Ensinger Tecatron® XP-87 Compression Molded PPS Compound, 20% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Surface Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |