Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00 - 1.00e+14 ohm | 1.00 - 1.00e+14 ohm | Average value: 1.28e+12 ohm Grade Count:43 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Surface Resistance | 1.00 - 1.00e+12 ohm | 1.00 - 1.00e+12 ohm | Average value: 6.17e+10 ohm Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Surface Resistance | 1.00 - 1.00e+6 ohm | 1.00 - 1.00e+6 ohm | Average value: 75200 ohm Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Surface Resistance | 1.00 - 1.00e+6 ohm | 1.00 - 1.00e+6 ohm | Average value: 252000 ohm Grade Count:27 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Surface Resistance | 1.00 - 1.00e+12 ohm | 1.00 - 1.00e+12 ohm | Average value: 1.44e+10 ohm Grade Count:92 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Surface Resistance | 1.00 - 1.00e+6 ohm | 1.00 - 1.00e+6 ohm | Average value: 79600 ohm Grade Count:20 |
Overview of materials for Polycarbonate, NCG Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Surface Resistance | 1.00 - 9.90e+11 ohm | 1.00 - 9.90e+11 ohm | Average value: 2.42e+9 ohm Grade Count:25 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Surface Resistance | 1.00 - 1.00e+6 ohm | 1.00 - 1.00e+6 ohm | Average value: 48800 ohm Grade Count:16 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
Surface Resistance | 1.00 - 1.00e+16 ohm | 1.00 - 1.00e+16 ohm | Average value: 8.14e+14 ohm Grade Count:69 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Surface Resistance | 1.00 - 1.00e+16 ohm | 1.00 - 1.00e+16 ohm | Average value: 9.40e+14 ohm Grade Count:113 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Surface Resistance | 1.00 - 1.00e+13 ohm | 1.00 - 1.00e+13 ohm | Average value: 2.00e+11 ohm Grade Count:40 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Surface Resistance | 1.00 - 1.00e+10 ohm | 1.00 - 1.00e+10 ohm | Average value: 4.17e+8 ohm Grade Count:28 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Surface Resistance | 1.00 - 1.00e+6 ohm | 1.00 - 1.00e+6 ohm | Average value: 117000 ohm Grade Count:10 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Surface Resistance | 1.00 - 1.00e+6 ohm | 1.00 - 1.00e+6 ohm | Average value: 319000 ohm Grade Count:18 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Surface Resistance | 1.00 - 5.20e+15 ohm | 1.00 - 5.20e+15 ohm | Average value: 1.28e+14 ohm Grade Count:230 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Surface Resistance | 1.00 - 100 ohm | 1.00 - 100 ohm | ASTM D257 |
Daelim H&L Plavis-C CM Conductive Polyimide Bearing Compression Molded. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grad.. |
|||
Surface Resistance | 1.00 - 100 ohm | 1.00 - 100 ohm | ASTM D257 |
Daelim H&L Plavis-C DF Conductive Polyimide Bearing Direct Formed. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grades:PL.. |
|||
Surface Resistance | 1.00 - 1.00e+16 ohm | 1.00 - 1.00e+16 ohm | Average value: 9.02e+14 ohm Grade Count:59 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Surface Resistance | 1.00 - 1.00e+6 ohm | 1.00 - 1.00e+6 ohm | Average value: 573000 ohm Grade Count:7 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Surface Resistance | 1.00 - 1.00e+7 ohm | 1.00 - 1.00e+7 ohm | Average value: 363000 ohm Grade Count:43 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Surface Resistance | 1.00 - 9.90e+11 ohm | 1.00 - 9.90e+11 ohm | Average value: 2.79e+10 ohm Grade Count:28 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |
|||
Surface Resistance | 1.00 - 1.60e+17 ohm | 1.00 - 1.60e+17 ohm | Average value: 5.70e+15 ohm Grade Count:271 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |