Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 400 - 1.00e+15 ohm-cm | 400 - 1.00e+15 ohm-cm | Average value: 7.50e+14 ohm-cm Grade Count:4 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Electrical Resistivity | 400 - 1.00e+16 ohm-cm | 400 - 1.00e+16 ohm-cm | Average value: 1.31e+15 ohm-cm Grade Count:29 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Electrical Resistivity | 400 ohm-cm | 400 ohm-cm | 5.3% graphite |
TIMCAL TIMREX® KC44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 400 ohm-cm | 400 ohm-cm | 5.4% graphite |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 400 ohm-cm | 400 ohm-cm | 5.5% graphite |
TIMCAL TIMREX® KS44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 400 ohm-cm | 400 ohm-cm | 4.9% graphite |
TIMCAL TIMREX® MB15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 400 ohm-cm @Temperature 130 °C |
400 ohm-cm @Temperature 266 °F |
ASTM D991 |
Borealis Low Sulfur™ LE0594 Crosslinkable Semiconductive Compound for Shielding of Power Cables Low Sulphur LE0594 is designed for use as a conductor and bonded insulation shield for medium and high voltage cables. LE0594 is a peroxide crosslinkable compound and is specifically intended to me.. |
|||
Electrical Resistivity | 400 ohm-cm | 400 ohm-cm | 4.9% graphite |
TIMCAL TIMREX® MB25 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 400 ohm-cm | 400 ohm-cm | |
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:.. |
|||
Electrical Resistivity | 400 ohm-cm @Temperature 130 °C |
400 ohm-cm @Temperature 266 °F |
ASTM D991 |
Borealis Low Sulfur™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables Low Sulphur LE0595 is designed for use as a conductor and bonded insulation shield for medium and high voltage cables. LE0594 is a peroxide crosslinkable compound and is specifically intended to me.. |