Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ Dipolymer, 22% Carbon Black Filled
(discontinued **) Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FE-5610Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FE-5620Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FE-5641Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FE-5660Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2110Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Viscosity .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2121 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2174 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2179 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2180 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Lower mold shrinkage and excellent co.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FE-5622Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2122 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good flow, release and hot tear for c.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2123 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent hot tear and compression se.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2144 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Higher viscosity version of FC-2123. .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2176 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good general purpose grade with good .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2177 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Slower cure rate and high tear streng.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2181 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Combines high elongation with excelle.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FLS-2530 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. High fluorine dipolymer with improved f.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2120 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for difficult extrusions. .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2182 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for autoclave curing. Used.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FG-5630Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2145 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2230 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2178 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Electrical Resistivity | 0.100 - 1.00e+14 ohm-cm | 0.100 - 1.00e+14 ohm-cm | Average value: 4.62e+13 ohm-cm Grade Count:13 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | Average value: 8.50e+13 ohm-cm Grade Count:6 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+14 ohm-cm | 1.00e+12 - 1.00e+14 ohm-cm | Average value: 5.35e+13 ohm-cm Grade Count:6 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+14 ohm-cm | 1.00e+12 - 1.00e+14 ohm-cm | Average value: 5.27e+13 ohm-cm Grade Count:4 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Electrical Resistivity | 1.00e+7 - 1.00e+14 ohm-cm | 1.00e+7 - 1.00e+14 ohm-cm | Average value: 4.32e+13 ohm-cm Grade Count:7 |
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+14 ohm-cm | 1.00e+11 - 1.00e+14 ohm-cm | Average value: 1.63e+13 ohm-cm Grade Count:22 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |