Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FE-5660Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2121 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FE-5622Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2123 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent hot tear and compression se.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2181 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Combines high elongation with excelle.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2145 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FC-2230 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+17 ohm-cm | 1.00e+13 - 1.00e+17 ohm-cm | Average value: 3.36e+16 ohm-cm Grade Count:6 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Electrical Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf.. |
|||
Electrical Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | |
Momentive Performance Materials RTV12 Clear General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 264E4861310 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE Butyrate 264E0096908 Natural, Trsp TENITE cellulosic plastic.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 550E4861316 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate Plasticizer 8%. Weight loss on heating = 0.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 360E0096907 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, .. |
|||
Electrical Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | ASTM D257 |
Chang Chun Plastic Longlite PM T355J Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Electrical Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | DIN 53482/VDE 0303 |
BASF Elastollan® C-64D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | Average value: 5.05e+14 ohm-cm Grade Count:45 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Acetate 109E3V36324 Clear, Trsp Cellulose Acetate
(discontinued **) Plasticizer 24%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 3.30e+17 ohm-cm | 1.00e+13 - 3.30e+17 ohm-cm | Average value: 2.04e+16 ohm-cm Grade Count:34 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | |
3M Dyneon™ Fluorel™ FG-5690Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia.. |