Polymer Property : Electrical Resistivity = 0.000136 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 0% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 900 °C
0.000136 ohm-cm

@Temperature 1650 °F
Haynes 625 alloy, 20% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 20% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 20% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 20% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 900 °C
0.000136 ohm-cm

@Temperature 1650 °F
Haynes 625 alloy, 20% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 20% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 30% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 30% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 50% cold reduction, 1010°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 50% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 900 °C
0.000136 ohm-cm

@Temperature 1650 °F
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 900 °C
0.000136 ohm-cm

@Temperature 1650 °F
Haynes 625 alloy, hot rolled and 1050°C mill-annealed plate
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 900 °C
0.000136 ohm-cm

@Temperature 1650 °F
Haynes 625 alloy, plate after 1000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, plate after 1000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 900 °C
0.000136 ohm-cm

@Temperature 1650 °F
Haynes 625 alloy, plate after 1000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, plate after 1000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, plate after 16000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, plate after 4000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, plate after 8000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000136 ohm-cm
0.000136 ohm-cm
Goodfellow Cobalt/Boron/Silicon/Iron/Molybdenum/Nickel Alloy
Information provided by Goodfellow.
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 30% cold reduction, 1010°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 900 °C
0.000136 ohm-cm

@Temperature 1650 °F
Haynes 625 alloy, 40% cold reduction, 1010°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 900 °C
0.000136 ohm-cm

@Temperature 1650 °F
Haynes 625 alloy, 50% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 50% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 400 °C
0.000136 ohm-cm

@Temperature 752 °F
Haynes 625 alloy, 10% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C (1500°F), good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a var..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 900 °C
0.000136 ohm-cm

@Temperature 1650 °F
Haynes 625 alloy, 10% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Electrical Resistivity 0.000136 ohm-cm

@Temperature 900 °C
0.000136 ohm-cm

@Temperature 1650 °F
Haynes 625 alloy, 40% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..