Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000130 ohm-cm @Temperature 500 °C |
0.000130 ohm-cm @Temperature 932 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 1000 °C |
0.000130 ohm-cm @Temperature 1830 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 1000 °C |
0.000130 ohm-cm @Temperature 1830 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 1000 °C |
0.000130 ohm-cm @Temperature 1830 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 1000 °C |
0.000130 ohm-cm @Temperature 1830 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 1000 °C |
0.000130 ohm-cm @Temperature 1830 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 1000 °C |
0.000130 ohm-cm @Temperature 1830 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 1000 °C |
0.000130 ohm-cm @Temperature 1830 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 1000 °C |
0.000130 ohm-cm @Temperature 1830 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 24.0 °C |
0.000130 ohm-cm @Temperature 75.2 °F |
|
Haynes Hastelloy® C-276 alloy, solution heat treated flat products Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
HP Alloys Alloy C-276, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
HP Alloys Alloy C-276, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
HP Alloys Alloy C-276, 40% Cold Worked 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
HP Alloys Alloy C-276, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725) Age Hardened Strip Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Strip samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Tube Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Age Hardened Tube samples. Other property values are typical of INCONEL® alloy 725.Data provi.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Round Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Round samples. Other property values are typical of INCONEL® alloy 725.Data provided.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Tube Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Tube samples. Other property values are typical of INCONEL® alloy 725.Data provided .. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
Goodfellow Cobalt/Silicon/Boron/Manganese Alloy Information provided by Goodfellow.Composition Notes: Si + B content = 25 wt%. Fe+Mo content = 2 wt%. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276 AL 276 alloy is a nickel-chromium-iron-tungsten alloy which is among the most corrosion resistant of alloys currently available. The AL 276 alloy is widely used in the severest environments encount.. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 1000 °C |
0.000130 ohm-cm @Temperature 1830 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
HP Alloys Alloy C-276, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 1 Cold Worked Level 1 Cold Worked applies to tensile properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 3 Cold Worked Level 3 Cold Worked applies to tensile properties of 0.25 to 2.4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
HP Alloys Nitronic® 60 Austenitic Stainless, Annealed Annealed applies to tensile and/or hardness; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was originally designed as a high tempe.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 4 Cold Worked Level 4 Cold Worked applies to tensile properties of 0.25 to 2 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |
|||
Electrical Resistivity | 0.000130 ohm-cm | 0.000130 ohm-cm | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 5 Cold Worked Level 5 Cold Worked applies to tensile properties of 0.25 to 1.5 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig.. |