Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000120 ohm-cm | 0.000120 ohm-cm | RT |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 704°C (1300°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Electrical Resistivity | 0.000120 ohm-cm | 0.000120 ohm-cm | RT |
Haynes Hastelloy® N, weld metal, aged 500 hours at 649°C (1200°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Electrical Resistivity | 0.000120 ohm-cm @Temperature 300 °C |
0.000120 ohm-cm @Temperature 572 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-28EH Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-28UH Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-30EH Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-30UH Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-35 Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-35H Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-35SH Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-38 Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-38SH Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-40M Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-40SH Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-42M Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-45 Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-45M Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-50 Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-30EZ Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-33H Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-33SH Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-38H Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-38M Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 - 0.000160 ohm-cm | 0.000120 - 0.000160 ohm-cm | |
Alliance N-48 Neodymium Iron Boron Magnetic Material |
|||
Electrical Resistivity | 0.000120 ohm-cm | 0.000120 ohm-cm | RT |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 593°C (1100°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Electrical Resistivity | 0.000120 ohm-cm | 0.000120 ohm-cm | RT |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 760°C (1400°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Electrical Resistivity | 0.000120 ohm-cm | 0.000120 ohm-cm | RT |
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Electrical Resistivity | 0.000120 ohm-cm | 0.000120 ohm-cm | |
HP Alloys HPA COBALT Alloy 6B, Wear Resistant, (Co-Cr-W) (UNS R30016) Cobalt 6B is a cobalt based chromium, tungsten alloy for wear environments where seizing, galling and abrasion are present. 6B is resistant to seizing and galling and with its low coefficient of fri.. |