Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000900 ohm-cm @Temperature 200 °C |
0.0000900 ohm-cm @Temperature 392 °F |
|
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Electrical Resistivity | 0.0000900 ohm-cm @Temperature 200 °C |
0.0000900 ohm-cm @Temperature 392 °F |
|
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Electrical Resistivity | 0.0000900 ohm-cm @Temperature 200 °C |
0.0000900 ohm-cm @Temperature 392 °F |
|
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Electrical Resistivity | 0.0000900 ohm-cm @Temperature 20.0 °C |
0.0000900 ohm-cm @Temperature 68.0 °F |
|
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resi.. |
|||
Electrical Resistivity | 0.0000900 ohm-cm @Temperature 20.0 °C |
0.0000900 ohm-cm @Temperature 68.0 °F |
|
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel Description: CLI SIRIUS S12 grade is an austenitic stainless steel containing 20% Cr, 1.8 % Si and 12% Ni. The low nickel content combined with high chromium and high silicon contents provide good r.. |
|||
Electrical Resistivity | 0.0000900 ohm-cm @Temperature 20.0 °C |
0.0000900 ohm-cm @Temperature 68.0 °F |
|
Industeel SIRIUS S15 Rare Earth Containing Heat Resistant Steel CLI SIRIUS S15 grade is a fully austenitic stainless steel containing 21 Cr, 1.7 Si, 0.17 N and Rare Earth elements (Cerium, Lanthanum,...etc) which make the alloy particularly well designed for hig.. |
|||
Electrical Resistivity | 0.0000900 ohm-cm @Temperature 20.0 °C |
0.0000900 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42 Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0... |
|||
Electrical Resistivity | 0.0000900 ohm-cm | 0.0000900 ohm-cm | |
Goodfellow Nickel 78/Boron 14/Silicon 8 Alloy Information provided by Goodfellow. |
|||
Electrical Resistivity | 0.0000900 ohm-cm @Temperature 200 °C |
0.0000900 ohm-cm @Temperature 392 °F |
|
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |