Processing Properties Metric English Comments
Melt Temperature 316 - 341 °C
601 - 646 °F
PolyOne Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Melt Temperature 316 - 341 °C
601 - 646 °F
PolyOne Therma-Tech™ LC-5000C TC LCP  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L 9512 PPS, 45% Glass Fiber  (discontinued **)
Good-flow Embedding Compound. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Embedding of Microchips and Electronic ComponentsProcessing: Injection Molding (Melt Temp..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L 9521-1 PPS, 60% Glass Fiber/Mineral  (discontinued **)
Extremely Rigid. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Sockets, Plugs and HandlesProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperatur..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L 9530 PPS, 55% Mineral  (discontinued **)
Good-flow Embedding Compound, Isotropic Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Embedding of Microchips and Electronic ComponentsProcessing: Inject..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L 9561 PPS, 60% Glass Fiber/Mineral  (discontinued **)
High Gloss, Highest Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Various High Temperature ReflectorsProcessing: Inje..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L V 9107-1 PPS, 40% Glass Fiber  (discontinued **)
Low Flash, Improved Impact and Burst Strength. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pump Housings, Hollow Articles Under PressureProcessing: Injection Moldi..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L V 9113-2 PPS, 60% Glass Fiber  (discontinued **)
Glass Fiber Grade with Highest Mechanical Strength and Stiffness. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Housings for Shock Absorbers and Spring ElementsProce..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L V 9200-1 PPS, 60% Glass Fiber/Mineral  (discontinued **)
Mineral-filled Grade with Improved Impact Strength, Low Mold Temp. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Shaft Seals, FlangesProcessing: Injection Molding (M..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L V 9300-1 PPS, 40% Glass Fiber/Glass Bead  (discontinued **)
Improved Impact Strength, Low Flash, Low Warpage. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Hollow Articles Under Pressure, Pump HousingsProcessing: Injection Mo..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L V 9400-1 PPS, 15% Carbon Fiber  (discontinued **)
High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Clutch Components, BushingsProcessing: Inje..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L 9511 PPS, 45% Glass Fiber
High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fixture Elements, HousingsProcessing: Injection Molding (Melt Temperature:..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L 9523 PPS, 60% Glass Fiber/Mineral
Extremely Rigid, Excellent Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Insulating Equipment, Reflectors and Fitting..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® P 9529 PPS, ~55% Glass Fiber/Mineral (black only)
Compounded Regrind and/or Production Scrap, Excellent Cost-Performance Ratio. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Lamp Holders, Lamp SocketsProcessing: Inj..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® P 9519 PPS, ~45% Glass Fiber (black only)
Compounded Regrind and/or Production Scrap, Excellent Cost-Performance Ratio. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Handles, Fixing ElementsProcessing: Injec..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L 9510-1 PPS, 40% Glass Fiber
High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pump Impellers, Valve Housings and BushingsProcessing: Injection Molding (..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L 9560 PPS, 50% Mineral
High Gloss, Highest Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Various High Temperature ReflectorsProcessing: Inje..
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Albis Plastics Tedur® L V 9404-1 PPS, 30% Carbon Fiber  (discontinued **)
High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fan Blades, Brake Sleeves, Model Constructi..
Melt Temperature 329 - 341 °C
624 - 646 °F
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry  (discontinued **)
Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..