Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 277 - 304 °C | 531 - 579 °F | |
PolyOne LubriOne™ NN-000/10T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 277 - 304 °C | 531 - 579 °F | |
PolyOne LubriOne™ NN-000/10T-2S Black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 277 - 304 °C | 531 - 579 °F | |
PolyOne LubriOne™ NN-000/15T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 277 - 304 °C | 531 - 579 °F | |
PolyOne LubriOne™ NN-000/20T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 282 - 304 °C | 540 - 579 °F | |
PolyOne Stat-Tech™ PC-15CF/000 Black Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 288 - 304 °C | 550 - 579 °F | |
PolyOne Stat-Tech™ NN-20CF/000 Black HS Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 288 - 304 °C | 550 - 579 °F | |
PolyOne Stat-Tech™ NN-20CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 282 - 304 °C | 540 - 579 °F | Stock |
PolyOne Edgetek® MP-10GF/000 Modified PPO - 10% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 160 - 304 °C | 320 - 579 °F | Average value: 200 °C Grade Count:27 |
Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Melt Temperature | 280 - 304 °C | 536 - 579 °F | |
BASF Ultramid® AZ HP UV BK 23220 PA66 (Dry) Description: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 o.. |
|||
Melt Temperature | 282 - 304 °C | 540 - 579 °F | Stock |
PolyOne Edgetek® MP-30GF/000 Modified PPO - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 20.0 - 304 °C | 68.0 - 579 °F | Average value: 274 °C Grade Count:22 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Melt Temperature | 271 - 304 °C | 520 - 579 °F | Stock |
PolyOne Lubri-Tech™ MP-15MCF/15T-2S Modified PPO - 15% Milled Carbon Fiber - 15% PTFE - 2% Silicone
(disconti Data provided by PolyOne. |