Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 249 - 266 °C | 480 - 511 °F | |
PolyOne Gravi-Tech™ GRV-PS-027-BA-WHT Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66BK Nylon 66 Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GF33BK Nylon 66, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GF33N Nylon 66, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GF43BK Nylon 66, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GF43N Nylon 66, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GF50BK Nylon 66, 50% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GM40BK Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GM40N Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 249 - 266 °C | 480 - 511 °F | |
LNP VALOX® SMV5845 PBT + PET Alloy, 16% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. Will be VC1600.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.Th.. |
|||
Melt Temperature | 249 - 266 °C | 480 - 511 °F | |
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement
(discontinued **) ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is .. |
|||
Melt Temperature | 249 - 266 °C | 480 - 511 °F | |
LNP VALOX® SMV5847 PBT + PET Alloy, 30% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. VC3000.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data .. |
|||
Melt Temperature | 238 - 266 °C | 460 - 511 °F | |
Styron EMERGEâ„¢ 7100 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7100 advanced resin exhibits a balance of properties between impact strength, heat resistance and processability. Its superior natural base color and lot-to-lot color .. |
|||
Melt Temperature | 226 - 266 °C | 439 - 511 °F | ISO 294 |
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 226 - 266 °C | 439 - 511 °F | ISO 294 |
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |