Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 300 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 149 - 171 °C
300 - 340 °F
ASTM D789
Niche Polymer PPCG30BK Copolymer PP, 30% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 149 - 171 °C
300 - 340 °F
ASTM D789
Niche Polymer PPCG40BK Copolymer PP, 40% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 149 - 171 °C
300 - 340 °F
ASTM D789
Niche Polymer PPCM10BK Copolymer PP
Information provided by Niche Polymer
Melt Temperature 149 - 171 °C
300 - 340 °F
ASTM D789
Niche Polymer PPCM6BK Copolymer PP
Information provided by Niche Polymer
Melt Temperature 149 - 232 °C
300 - 450 °F
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for..
Melt Temperature 149 - 232 °C
300 - 450 °F
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for..
Melt Temperature 149 - 279 °C
300 - 534 °F
Average value: 219 °C Grade Count:177
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Melt Temperature 149 - 232 °C
300 - 450 °F
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC1390AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC1390 is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density po..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC1550AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC1550 is used for extrusion-coating applications, especially when increased heat-seal range is needed.Application/UsesFlexible medicalFoilFood packagingFood-contac..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC1924AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC1924 is a resin that is widely used in the boardstock coating industry. This material has an excellent combination of low neck-in, ease of processing, good chill-..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC4041AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC4041 is recommended for use in the boardstock coating industry. The resin has low neck-in and good drawdown characteristics. Coatings produced from EC4041 have ex..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC4056AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC4056 is a natural low density material with an 80 melt index.FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All in..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC800AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC800 is a general-purpose low-density formulation used for extrusion coating applications.Application/UsesGeneral extrusion coatingFDA: This material complies with..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC808AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC808 is a general-purpose formulation used for injection molding, general-purpose extrusion coating and laminating. It can be drawn down to low coating weights, is..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC811AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC811 is used for extrusion coating applications. It exhibits good adhesion, low coat weight, and fast heat seals.Application/UsesCoatings for paper/paperboardFDA: ..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EC812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC812 is a natural low-density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a backing to carpet to bin..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM182AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM182 is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM184AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM184 is a low density injection-molding formulation suggested for the production of closures where a high melt index is needed to meet shrinkage requirements and f..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM1870AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM1870 is used for injection molding applications. It has excellent stress crack resistance for lids.Application/UsesFlexible medicalLidsMedicalFDA: This material c..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM808AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM808 is a general-purpose low-density formulation used for injection molding applications and general purpose extrusion.Application/UsesFood packagingMedicalFDA: T..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM811AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM811 is a low-density polyethylene used for injection molding. It is characterized by high flow and low stiffness.Application/UsesFlexible medicalMedicalFDA: This ..
Melt Temperature 149 - 166 °C
300 - 330 °F
Westlake EM812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM812 is a low-density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi..
Melt Temperature 149 °C
300 °F
Axiall 47551 Flexible PVC
Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 149 - 232 °C
300 - 450 °F
Average value: 193 °C Grade Count:3
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min..
Melt Temperature 149 - 310 °C
300 - 590 °F
Average value: 221 °C Grade Count:81
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..
Melt Temperature 149 °C
300 °F
Axiall 46234B Flexible PVC
Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 149 °C
300 °F
Axiall 4750 Flexible PVC
General purpose molding and extrusion compound well suited for automotive floor mats.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 149 - 240 °C
300 - 464 °F
Average value: 184 °C Grade Count:40
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
Melt Temperature 149 - 204 °C
300 - 400 °F
Ecomass® 5100TU96 Tungsten Filled SEBS
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled SEBS Base ResinVery FlexibleInformation provided by Technical..