Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 2580 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistanceApplications: Cutlery, Consumer electronicsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optic.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 602 Crystal Polystyrene GP Grade
(discontinued **) Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise spe.. |
|||
Melt Temperature | 168 - 274 °C | 335 - 525 °F | Average value: 221 °C Grade Count:17 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1290 High Heat Crystal Polystyrene Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3100 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5511 High Impact Polystyrene Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 6200 Super High Impact Polystyrene Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined.. |
|||
Melt Temperature | 218 - 274 °C | 424 - 525 °F | |
Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin TOTAL Petrochemicals Polypropylene LX5 02-15 is an experimental grade of isostatic polypropylene copolymer produced via TOTAL proprietary metallocene catalyst technology.Benefits. LX5 02-15 produc.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3510 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5460 High Impact Polystyrene
(discontinued **) High impact, Good environmental stress crack resistance, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on inject.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5620 High Impact Polystyrene
(discontinued **) High heat resistance, Good balance of toughness and rigidityApplications: Food service itemProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.I.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5470 High Impact Polystyrene
(discontinued **) High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection molded specimens at 23°C and.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 4501 Medium Impact Polystyrene
(discontinued **) Good toughnessApplications: Light louvers, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provide.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5504 High Impact Polystyrene
(discontinued **) Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio.. |