Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 182 - 191 °C | 360 - 376 °F | |
PolyOne Geon™ Vinyl Wire & Cable EMB405LB Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 182 - 191 °C | 360 - 376 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1349L NAT 0000 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 182 - 191 °C | 360 - 376 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1349L-xx09FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 185 - 191 °C | 365 - 376 °F | |
PolyOne Geon™ Vinyl Wire & Cable W2403 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 182 - 191 °C | 360 - 376 °F | |
PolyOne Geon™ Vinyl Cellular E8202 Polyvinyl Chloride, Rigid (PVC, Rigid) All physicals were measured on an actual extruded part of a shutter profile.High rate inward foam applications.Density range .55-.70.Information provided by PolyOne |
|||
Melt Temperature | 179 - 191 °C | 354 - 376 °F | |
PolyOne Geon™ Vinyl Flexible A48248D Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 191 °C | 354 - 376 °F | |
PolyOne Geon™ Vinyl Flexible A5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 185 - 191 °C | 365 - 376 °F | |
PolyOne Geon™ Vinyl Flexible R132BE Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Melt Temperature | 185 - 191 °C | 365 - 376 °F | |
PolyOne Geon™ Vinyl Flexible R148AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 191 °C | 360 - 376 °F | |
PolyOne Geon™ Vinyl Flexible R157AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 191 °C | 354 - 376 °F | |
PolyOne Geon™ Vinyl Flexible R1700E Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 191 °C | 354 - 376 °F | |
PolyOne Geon™ Vinyl Flexible R290AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 191 °C | 360 - 376 °F | |
PolyOne Geon™ Vinyl Flexible XV3881 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 191 °C | 360 - 376 °F | |
PolyOne Geon™ Vinyl Flexible F78E Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 185 - 191 °C | 365 - 376 °F | |
PolyOne Geon™ Vinyl Flexible R4294U Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 185 - 191 °C | 365 - 376 °F | |
PolyOne Geon™ Vinyl Flexible R4294W Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 191 °C | 350 - 375 °F | Extrusion |
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri.. |
|||
Melt Temperature | 177 - 191 °C | 350 - 375 °F | |
Sylvin Technologies 9077-75C Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 177 - 191 °C | 350 - 375 °F | |
Sylvin Technologies 9604-80C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 177 - 191 °C | 350 - 375 °F | |
Sylvin Technologies 9604-85C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 185 - 191 °C | 365 - 376 °F | |
PolyOne Geon™ Vinyl Flexible R339AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 191 °C | 351 - 376 °F | |
PolyOne Geon™ Vinyl Flexible R350AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 191 °C | 350 - 375 °F | |
Sylvin Technologies 9604-95C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 182 - 191 °C | 360 - 376 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1349L-xx05FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |