Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 365 - 385 °C | 689 - 725 °F | |
LATI LARPEEK 10 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 365 - 385 °C | 689 - 725 °F | |
LATI LARPEEK 10 K/20 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 365 - 385 °C | 689 - 725 °F | |
LATI LARPEEK 10 K/30 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 365 - 385 °C | 689 - 725 °F | |
LATI LATILUB 88/50-20GRT K/10 PEEK Based, 10% Carbon Fiber Reinforced, 20% Graphite and PTFE Self Lubricating Plastic Latilub self-lubricating plastic materials are designed to replace metals in applications such as gears, bushings, cams, slides, etc., for which, besides their intrinsic properties (moldability, low.. |
|||
Melt Temperature | 365 - 385 °C | 689 - 725 °F | |
LATI LATILUB 88/50-30GRT PEEK Based, 30% Graphite and PTFE Self Lubricating Plastic
(Unverified Data**)&l Latilub self-lubricating plastic materials are designed to replace metals in applications such as gears, bushings, cams, slides, etc., for which, besides their intrinsic properties (moldability, low.. |
|||
Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng.. |
|||
Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK) AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava.. |
|||
Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The .. |
|||
Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
Melt Temperature | 365 - 375 °C | 689 - 707 °F | |
E-Polymers SEPAZ® C230GI 30% Glass Fiber Reinforced Good Impact LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Melt Temperature | 365 - 390 °C | 689 - 734 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |