Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 238 - 266 °C | 460 - 510 °F | |
Ravago Manufacturing Americas Hylon® N2000HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 238 - 266 °C | 460 - 510 °F | Molding |
PolyOne Lubri-Tech™ PS-15GB/15T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 238 - 279 °C | 460 - 535 °F | |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Melt Temperature | 238 - 268 °C | 460 - 515 °F | |
Polymer Resources NY6-IM1 Nylon 6, Impact Modified Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (.. |
|||
Melt Temperature | 238 - 288 °C | 460 - 550 °F | |
DuPont Bexloy® AXW504BK Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | Injection |
Samsung Cheil Industries Starex® HF-5330S ASA, Unreinforced
(discontinued **) Amorphous Styrene Acrylonitrile (SAN)Characteristics: Heat Resistant: Impact and Chemical Resistance, Surface GlossApplications: Oil Filter Case, Lubricant Can, Refrigerator and Hair Dryer Component.. |
|||
Melt Temperature | 238 - 271 °C | 460 - 520 °F | Injection Molding |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
MTI ThermoStran® TPU-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
Clariant Renol PA2SP0008HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Melt Temperature | 238 °C | 460 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 238 - 282 °C | 460 - 540 °F | Average value: 256 °C Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |