Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 168 - 177 °C | 334 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0850-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 168 - 177 °C | 334 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0860-xx02D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 168 °C | 334 °F | |
PolyOne Geon™ Vinyl Wire & Cable JAB40L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Wire & Cable JJX20A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1104L-xx60FRDUV Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJX206L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible A6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible B65B1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible B65F1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 171 °C | 334 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJAF111L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible C6501 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible C6502 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 177 °C | 334 - 351 °F | |
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8925-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8940-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8950-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8980-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8999-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9940-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9950-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9980-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3302-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3311-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 90-A472R-60-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3211-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 59996J Moldings & Extrusions Flexible PVC Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 1651 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 10705 Wire & Cable Flexible PVC Non-lead stabilized general purpose 75C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 10757 Wire & Cable Flexible PVC General purpose non-lead stabilized 75°C rated compound recommended for jacketing and general purpose extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporati.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 22750 Coax & Telecom Flexible PVC Non-staining extrusion compound recommended for retractile telecommunication cord. Maximum service temperature of 60°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |