Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0800-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1104L-xx61FRD Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information p.. |
|||
Melt Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable JKC30A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable JLK51L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable MJF114A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1104L-xx40D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1250L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJX207L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 176 °C | 331 - 349 °F | |
PolyOne Geon™ Vinyl Wire & Cable Y594B Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Flexible R295AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Flexible R7542X Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Flexible SL60 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable WR3792CL Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 193 °C | 331 - 379 °F | Blown Film |
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: This SBC is easily processed on blown film or cast fi.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8940-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8980-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9604-80 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9940-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9950-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9980-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3300-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3301-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3310-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Melt Temperature | 166 - 193 °C | 331 - 379 °F | Blown Film |
Chevron Phillips K-Resin® DK11 Styrene-Butadiene Copolymer, Film Grade Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: Provides the same high performance film properties as.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 14750 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 2134N Moldings & Extrusions Flexible PVC 105C plug molding compound. UL recognized component for 94 V-2 in all colors (0.75 mm min. thickness) and 94 V-0 in black and white (1.5 mm min. thickness). UL QMFZ2 recognized component.Informati.. |
|||
Melt Temperature | 166 - 204 °C | 330 - 400 °F | |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melt Temperature | 166 - 204 °C | 330 - 400 °F | |
M. Holland Company MAGMA® LM311-D LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melt Temperature | 166 - 193 °C | 331 - 379 °F | Blown Film |
Chevron Phillips K-Resin® DK13 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: DK13 is an SBC designed for the film market and has i.. |