Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 154 - 160 °C | 309 - 320 °F | |
PolyOne Geon™ Vinyl Wire & Cable 3201-xx05D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable JJK501L Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable W2301 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJKC304 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 °C | 309 °F | ASTM D789 |
Niche Polymer PA66GF13BK Nylon 66, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJKC302LR Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 °C | 309 °F | |
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vica.. |
|||
Melt Temperature | 154 °C | 309 °F | |
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica.. |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Flexible R5160A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 154 - 210 °C | 310 - 410 °F | Average value: 181 °C Grade Count:157 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8600-60 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8915-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8925-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8940-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8950-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8960-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8980-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8999-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9600-60 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9915-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9925-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9940-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9950-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9960-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9980-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9999-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 °C | 310 °F | |
Spartech E65060 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Melt Temperature | 154 °C | 310 °F | |
Axiall 50896 Moldings & Extrusions Flexible PVC Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 154 °C | 310 °F | |
Teknor Apex APEX® 3200-45 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Melt Temperature | 154 - 213 °C | 310 - 415 °F | Average value: 179 °C Grade Count:121 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |