Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 143 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 143 - 171 °C
289 - 340 °F
PolyOne Versaflex™ CL2003X Thermoplastic Elastomer (TPE)
Versaflex™ CL2003X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and ultra-soft properties are desired. New Product. Commercial specifications ha..
Melt Temperature 143 - 154 °C
289 - 309 °F
Huntsman PE1058 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional draw down and processability, excellent strength, good heat sealability, and optics.Applications: Film extrusion: all thin film uses and especiall..
Melt Temperature 143 - 154 °C
289 - 309 °F
Huntsman PE1068 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional draw down and processability even to 1/2 mil; excellent strength, good heat sealability, and good optical.FDA Notes: Conforms to FDA regulation 21..
Melt Temperature 143 °C
290 °F
Spartech E65350 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Melt Temperature 143 °C
290 °F
Spartech E65450 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Melt Temperature 143 °C
290 °F
Spartech E65550 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Melt Temperature 143 °C
290 °F
Spartech E65650 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Melt Temperature 143 °C
290 °F
Spartech M60450 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 216 °C
290 - 420 °F
Processing
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Melt Temperature 143 - 216 °C
289 - 421 °F
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Melt Temperature 143 - 216 °C
289 - 421 °F
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Melt Temperature 143 - 216 °C
289 - 421 °F
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Melt Temperature 143 - 216 °C
289 - 421 °F
Processing
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer
A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Melt Temperature 143 - 216 °C
290 - 420 °F
Processing
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance ..