Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 749 - 799 °C | 1380 - 1470 °F | Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 230 HB |
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel Description: Thermodur® 2344 Magnum is an electro slag remelted (ESR) hot work die steel, designed to meet all die casting industry specificationCharacteristics: Excellent toughness; Excellent re.. |
|||
Annealing Temperature | 749 - 799 °C | 1380 - 1470 °F | Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 230 HB |
Schmolz + Bickenbach Thermodur® 2365 EFS Extra Fine Structure - Hot Work Die Steel Description: Thermodur® 2365 is an Extra Fine Structure (EFS) hot work tool steel developed for good high temperature strength and tempering resistance and Supplied in the annealed conditionChara.. |
|||
Annealing Temperature | 699 - 799 °C @Time 3600 sec |
1290 - 1470 °F @Time 1.00 hour |
Soft; Air cool |
Schmolz + Bickenbach UgiPermâ„¢ 12FM Stainless Steel Bar Description: UgiPermâ„¢ 12FM is a 12% chrome ferritic stainless with improved magnetic properties designed for use in electro-injectors, valves and many other applications. The grade was develope.. |
|||
Annealing Temperature | 760 - 799 °C | 1400 - 1470 °F | Soft; Cooling: Furnace 20°F/hour to 1200 °F/ Then air cooled; < 230 HB |
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi.. |
|||
Annealing Temperature | 750.0 - 799 °C | 1382 - 1470 °F | Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 230 HB |
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel Description: Thermodur® 2343 is a single melt Extra Fine Structure (EFS) hot work die steel and Supplied in the annealed conditionCharacteristics: Good toughness; Moderate high-temperature strength.. |
|||
Annealing Temperature | 749 - 799 °C | 1380 - 1470 °F | Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 230 HB |
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed conditionCharacteristics: Good toughness; Good resistance to thermal shock a.. |