Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel

Category Metal , Ferrous Metal , Tool Steel , Hot Work Steel
Manufacturer Schmolz + Bickenbach (Swiss Steel International)
Trade Name Thermodur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed conditionCharacteristics: Good toughness; Good resistance to thermal shock and fatigue; Good hardenability; and Good high-temperature strengthApplications: Hot forging dies, Hot extrusion tooling, Forming dies, Plastic molds and Shot sleeveStress Relieving (Heat Treatment): 1200°F for 2 hours; Cooling: Cool slowly to 930°F in air; Hardness:
Physical Properties Metric English Comments
Density 7.78 g/cc
0.281 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 34

@Treatment Temp. 700.0 °C,
Time 7200 sec
34

@Treatment Temp. 1292 °F,
Time 2.00 hour
42

@Treatment Temp. 650.0 °C,
Time 7200 sec
42

@Treatment Temp. 1202 °F,
Time 2.00 hour
50

@Treatment Temp. 600.0 °C,
Time 7200 sec
50

@Treatment Temp. 1112 °F,
Time 2.00 hour
54

@Treatment Temp. 400 °C,
Time 7200 sec
54

@Treatment Temp. 752 °F,
Time 2.00 hour
54

@Treatment Temp. 550.0 °C,
Time 7200 sec
54

@Treatment Temp. 1022 °F,
Time 2.00 hour
56

@Treatment Temp. 500 °C,
Time 7200 sec
56

@Treatment Temp. 932 °F,
Time 2.00 hour
Tensile Strength 1320 MPa
192000 psi
42 HRC
1670 MPa
242000 psi
50 HRC
1790 MPa
259000 psi
52 HRC
Thermal Properties Metric English Comments
CTE, linear 10.8 µm/m-°C

@Temperature 21.1 - 93.3 °C
6.00 µin/in-°F

@Temperature 70.0 - 200 °F
11.9 µm/m-°C

@Temperature 21.1 - 204 °C
6.60 µin/in-°F

@Temperature 70.0 - 400 °F
12.6 µm/m-°C

@Temperature 21.1 - 399 °C
7.00 µin/in-°F

@Temperature 70.0 - 750 °F
Thermal Conductivity 25.5 W/m-K

@Temperature 21.1 °C
177 BTU-in/hr-ft²-°F

@Temperature 70.0 °F
27.5 W/m-K

@Temperature 343 °C
191 BTU-in/hr-ft²-°F

@Temperature 650 °F
30.3 W/m-K

@Temperature 704 °C
210 BTU-in/hr-ft²-°F

@Temperature 1300 °F
Component Elements Properties Metric English Comments
Carbon, C 0.40 %
0.40 %
Chromium, Cr 5.3 %
5.3 %
Iron, Fe 90.9 %
90.9 %
Molybdenum, Mo 1.4 %
1.4 %
Silicon, Si 1.0 %
1.0 %
Vanadium, V 1.0 %
1.0 %
Processing Properties Metric English Comments
Annealing Temperature 749 - 799 °C
1380 - 1470 °F
Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 230 HB