Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 6.00 Month | 6.00 Month | |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Shelf Life | 6.00 Month @Temperature 25.0 °C |
6.00 Month @Temperature 77.0 °F |
|
Lord Adhesives Fusor® 380NS / 383NS Epoxy Adhesive LORD Fusor® 380NS/383NS adhesive is a two-part, rapid-cure epoxy adhesive used to bond fiberglass reinforced plastics (FRP), sheet molded compounds (SMC) and metals.All information provided by Lo.. |
|||
Shelf Life | 6.00 Month @Temperature -40.0 °C |
6.00 Month @Temperature -40.0 °F |
|
Lord Adhesives Thermosetâ„¢ ME-542 Underfill Encapsulant LORD Thermosetâ„¢ ME-542 encapsulant is an anhydridefree, thermally conductive, semiconductor grade epoxy underfill product developed for the encapsulation of densely populated area array flip ch.. |
|||
Shelf Life | 6.00 Month | 6.00 Month | with proper storage |
Stanelco Bioplast® GS 2189 Biodegradable Plastic Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable i.. |
|||
Shelf Life | 6.00 Month | 6.00 Month | in original unopened containers |
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi.. |
|||
Shelf Life | 6.00 Month @Temperature 21.1 °C |
6.00 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 19146R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Black silicone gum and rubber on fiberglass clothT.. |
|||
Shelf Life | 6.00 Month @Temperature 7.22 °C |
6.00 Month @Temperature 45.0 °F |
|
Arlon 25188T020 0.020" Uncured Silicone Rubber/Laminated ETFE Film Design/Construction:Liner: 0.003" PTFE Coated FiberglassSide 1: Uncured Silicone RubberSubstrate: Laminated ETFE Film-treated for adhesionThis data represents typical values for the production ma.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 30090R022 0.022" (0.559 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The d.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 32140R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 49581R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 51576R024A 0.024" (0.610 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 51586R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clot.. |
|||
Shelf Life | 6.00 Month @Temperature 21.1 °C |
6.00 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 51581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu.. |
|||
Shelf Life | 6.00 Month @Temperature 18.3 - 23.9 °C |
6.00 Month @Temperature 65.0 - 75.0 °F |
From date of manufacture |
Arlon 51591R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data .. |
|||
Shelf Life | 6.00 Month @Temperature 21.1 °C |
6.00 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 55578R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPESide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Silicone Skim Coat Appearance: Red silico.. |
|||
Shelf Life | 6.00 Month | 6.00 Month | From date of manufacture |
Arlon 55578XC028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Shelf Life | 6.00 Month @Temperature <=26.7 °C |
6.00 Month @Temperature <=80.1 °F |
|
3M AC-360 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-360 Class B are fast cure, intermediate density two-component, manganese dioxide cure, polysulfide fuel tank and fuselage sealant. 3M AC-360 Class B Sealants have outstanding.. |
|||
Shelf Life | 6.00 Month @Temperature 21.1 °C |
6.00 Month @Temperature 70.0 °F |
|
Arlon R35551X015 0.015" Uncured Silicone Rubber with Woven Fabric Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Primed 3M Nextel 312 Woven Fabric AF-10, HCSide 2: Uncured Silicone RubberThis data represents typica.. |
|||
Shelf Life | 6.00 Month | 6.00 Month | in tightly closed container |
BCC Products BC 4553 Polyester Styling Paste BC4553 is designed for instant buildup and repair of plastic surfaces and models. Recommended for use on SMC and FRP parts, vacuum form molds and a variety of surfaces. When cured BC4553 produces a .. |
|||
Shelf Life | 6.00 Month | 6.00 Month | |
Aremco Ceramabind™ 644-A High Temperature Inorganic Binder An acidic, colloidal alumina binder developed for mixing with sized refractory flours and grains to produce high temperature refractory coatings for ceramic fiber boards. Used as a superior standalo.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 44571R010A 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
|
Arlon 51426R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the pr.. |
|||
Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
|
Arlon 55141R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Shelf Life | 6.00 Month | 6.00 Month | |
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F. |
|||
Shelf Life | 6.00 Month | 6.00 Month | Unopened Container |
Parker Chomerics Tecknit® 73-00025 Electrically Conductive Acrylic and Polyurethane Paint Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosure.. |
|||
Shelf Life | 6.00 Month @Temperature 21.1 °C |
6.00 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon R37500G060 0.060" (1.52 mm) Uncured Fluorosilicone with Release PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Fluorosilicone Carrier: Release PETThis data represents typical values for the production material. The data should not be used to write,.. |
|||
Shelf Life | 6.00 Month @Temperature 21.1 °C |
6.00 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 32210A005 0.005" (0.127 mm) Uncured Fluorosilicone Rubber on Polyester Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Fluorosilicone RubberCarrier: PolyesterThis data represents typical values for the production material. The data should not be used to wr.. |