Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 15.0 Month | 15.0 Month | Unopened Container |
Parker Chomerics Tecknit® 72-00008 Silver-Filled Epoxy System Description: This commercial grade, conductive epoxy is designed for use in bonding applications where good conductivity is required. When mixed in a ratio of 1:1.4 by volume or weight, the two comp.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | Unopened Container |
Parker Chomerics Tecknit® 72-08116 Silver-Filled Epoxy System Description: This is a silver filled epoxy system designed for maximum performance and lowest volume resistivity. It is easily mixed 1:1 by volume or weight, from the two one-ounce jars. Its consist.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Borealis Visico™/Ambicat™ LE4421/LE4472 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4472 is a silane crosslinkable black compound designed for covering/insulation of overhead cables. The base material Visico™ LE4421 in combination with the catalyst m.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning 739 PLASTIC ADHESIVE One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB, good adhesion.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SE 1896 FR KIT Two-part, translucent, heat cure.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® 9251/45 A&B KIT 45 Durometer, 2-part, 1 to 1 mix, off-white, Fabric Coating grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® 9280/60E KIT PARTS A&B 75 Shore A hardness, two-part, 1 to 1 mix, translucent, injection molding grade Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® 9280/70E KIT PARTS A&B 70 Durometer, 2 parts, 1 to 1 mix, translucent, injection molding grade Liquide Silicone Rubber.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® 9280/75E KIT PARTS A&B 60 Durometer, 2-part, 1 to 1 mix, translucent, injection moulding grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® 9412/30E KIT PARTS A&B 30 Durometer, 2-part, 1 to 1 mix, 2-part, 1 to 1 mix, opaque, Auto connector seal grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® 9412/50E KIT PARTS A&B 50 Durometer, 2-part, 1 to 1 mix, opaque, Auto connector seal grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® 9414/50E KIT PARTS A&B 50 Durometer, 2-part, 1 to 1 mix, opaque, Auto connector seal grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® 9416/30E KIT PARTS A&B 30 Durometer, two-part, 1 to 1 mix, opaque, injection mold grade silicone rubber.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® 9416/50 KIT PARTS A&B 50 Durometer, 2-part, 1 to 1 mix, opaque, Auto connector seal grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® LSR 9390-40 PARTS A&B 40 Durometer, 2-part, 1 to 1 mix, off-white, molding grade, Liquid Silicone RubberInformation provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning SILASTIC® LSR 9390-60 PARTS A&B 60 Durometer, 2-part, 1 to 1 mix, oil resistant, tan Liquid Silicone Rubber for injection molding.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning XIAMETER® PMCPMEM-1171 Emulsion Is chemically equivalent to DOW CORNING® 2-1171 EMULSION. Non-ionic, 50% emulsion of polydimethylsiloxane.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning Z-6172 SILANE Dow Corning® Z-6172 Silane is an organofunctional reactive silane. The product has a vinyl reactive organic group and a 2-methoxyethoxysilyl reactive inorganic group. Dow Corning® Z-6172 Silane ha.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning Z-6187 SILANE Dow Corning® Z-6187 Silane is a dialkyldimethoxysilane. Silanes and siloxanes have been used for some time in this application to increase yield and improve the stereoregularity of the polyolefin r.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning 2-1171 EMULSION Dow Corning® 2-1171 Emulsion is a milky white emulsion of polydimethylsiloxane. This nonionic emulsion contains 50 percent silicone.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning XIAMETER® PMCPMEM-0037 Emulsion Is chemically equivalent to DOW CORNING® 37 EMULSION. Anionic, 35% active emulsion based on high viscosity polydimethylsiloxane.Information provided by Dow Corning |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning 36 EMULSION Non-ionic, 35% active, emulsion of a medium viscosity trimethylsilyl terminated polydimethylsiloxane. This product has been replaced by Dow Corning® IE 39 EmulsionInformation provided by Dow Cornin.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
3M 800 Industrial Sealant 3M™ Scotch-Seal™ Industrial Sealant 800 is a reddish brown, brushable sealant that air dries to a flexible seal that resists water, oils and fuel and adheres to many metallic surfaces and has a us.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
3M Fastbond™ 4213-NF Industrial Adhesive 3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
3M Scotch-Weld™ 4475 Industrial Adhesive Features: Dries quickly to a firm bondExcellent resistance to water, plasticizer migration, many detergent and soap solutions, oils and greasesA general purpose adhesive for bonding most vinyls, cer.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
3M Weatherban™ 606NF Acrylic Sealant 3M™ Weatherban™ Acrylic Sealant 606NF is a bright, white, premium quality, water-based paintable sealant.Features:Water-basedPaintableWeather resistantConstruction, maintenance repair operation (M.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Parker Chomerics CHO-SHIELD® 1091 Adhesion Promoter for Conductive Polyurethane Coatings Information provided by Chomerics |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
3M Scotch-Weld™ 2262 Plastic Adhesive Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very .. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Dow Corning DSP ANTIFOAM EMULSION 10 percent active silicone emulsion that exhibits outstanding dilution stability as well as excellent foam control persistance over a wide pH and temperature range.Information provided by Dow Cornin.. |
|||
Shelf Life | 15.0 Month | 15.0 Month | |
Borealis Visico™/Ambicat™ LE4421/LE4476 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4476 is a silane crosslinkable natural compound designed for low voltage power cables up to 6kV. The base material Visico™ LE4421 in combination with the catalyst mas.. |