Dow Corning SILASTIC® 9251/45 A&B KIT

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 9251/45 A&B KIT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
45 Durometer, 2-part, 1 to 1 mix, off-white, Fabric Coating grade, Liquid Silicone Rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc

@Temperature 25.0 °C
1.22 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Viscosity 80000 cP
80000 cP
mixing, dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 42
42
Tensile Strength, Ultimate 6.00 MPa
870 psi
Elongation at Break 430 %
430 %
Tear Strength 9.99 kN/m
57.0 pli
Electrical Properties Metric English Comments
Volume Resistivity 3.10e+15 ohm-cm
3.10e+15 ohm-cm
Processing Properties Metric English Comments
Pot Life 4320 min
4320 min
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Color off-white
Mix Ratio (X:1) 100
Base to Catalyst ETN