Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 12.0 Month | 12.0 Month | Normal Storing Conditions |
Premix Thermoplastics PREBLACK PE 704-40 PREBLACK PE 704-40 black masterbatch has been developed for the coloring of PE-LD, PE-LLD and PE-HD films when maximum UV-resistance and pureness is required.The moisture absorption of PREBLACK PE 7.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | Normal Storing Conditions |
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Permabond POP Polyolefin Primer Permabond® Polyolefin Primer has been developed for surface treatment of polyolefins, PTFE and silicones prior to bonding with Permabond® Cyanoacrylate adhesives. Due to their low surface energy, .. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Permabond 931 Cyanoacrylate PERMABOND 931 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Shelf Life | 12.0 Month @Temperature 25.0 °C |
12.0 Month @Temperature 77.0 °F |
|
Lord Adhesives Metech 1130C Platinum Silver Conductor Composition This low cost, platinum silver conductor is designed for general hybrid applications. It employs advanced powders technology with a mix bonded frit system to yield a highly dense film that is resist.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Solvay AG-RHOâ„¢ EM 30 Surfactant Description: High performance emulsifier for methylated and natural seed oils. Excellent emulsion stability in a wide range of water hardness.Identification: AGRICULTURAL EMULSIFIER BLENDWater Solub.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Solvay RHODACAL® SS-45/A2 Surfactant Identification: SODIUM ALKYL BENZENE SULFONATECAS: 68081-81-2 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODACAL SS-45/A2 is product that is especially suitabl.. |
|||
Shelf Life | 12.0 Month @Temperature 23.9 °C |
12.0 Month @Temperature 75.0 °F |
in unopened containers |
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one .. |
|||
Shelf Life | 12.0 Month | 12.0 Month | 35-45°F |
Master Bond MB297FL Cyanoacrylate Adhesive System Vibration & shock resistant, fills gap to 0.007Information provided by Master Bond Inc. |
|||
Shelf Life | 12.0 Month @Temperature -40.0 °C |
12.0 Month @Temperature -40.0 °F |
|
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive TRA-BOND 789-3 one component, high strength toughened adhesive is designed for microelectronic applications, including substrate attach and package sealing, which require good moisture resistance. I.. |
|||
Shelf Life | 12.0 Month @Temperature -18.0 °C |
12.0 Month @Temperature -0.400 °F |
|
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix HexPly® M42 is a high performance, self extinguishing, self adhesive, tough epoxy matrix for use in primary aerospace sandwich structures. It exhibits very high impact resistance and damage toleran.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning FLUOROGEL® Q3-6679 DIELECTRIC GEL KIT Two-part, clear, RT or heat cure, solvent and fuel resistant.Information provided by Dow Corning |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning Q3-3559 SEMIFLOWABLE TEXTILE ELASTOMER A semi-flowable 1 part solventless silicone elastomer.Information provided by Dow Corning |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning SYL-OFF® 7362 COATING Syl-Off® 7362 Coating is a 30% solids dispersion of vinyl functional silicone polymer in toluene. A pre-catalysed coating suitable for fast cure applications, recommended for use with 7367 Crosslin.. |
|||
Shelf Life | 12.0 Month @Temperature 25.0 °C |
12.0 Month @Temperature 77.0 °F |
|
Epoxy Technology EPO-TEK® 353ND-T5 High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T5 is an intermediate viscosity version of EPO-TEK® 353ND and EPO-TEK® 353ND-T. It was designed for high temperature applications in fiber optics, electronics .. |
|||
Shelf Life | 12.0 Month @Temperature 25.0 °C |
12.0 Month @Temperature 77.0 °F |
|
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning 1437 INDUSTRIAL SEALANT AND ADHESIVE Neutral Cure RTV SealantInformation provided by Dow Corning |
|||
Shelf Life | >= 12.0 Month | >= 12.0 Month | |
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR) SE BR-1220L is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low ash content. A non-staining stabilizer is added during the production.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Dow Corning 3-3442 FLOWABLE TEXTILE SEALANT A flowable one part acid curing rtv silicone for elastomeric coatings.Information provided by Dow Corning |
|||
Shelf Life | 12.0 Month @Temperature 21.1 °C |
12.0 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 920-05B##-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular 0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Sel.. |
|||
Shelf Life | 12.0 Month @Temperature 23.9 °C |
12.0 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon LW201Xxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Shelf Life | 12.0 Month @Temperature 5.00 - 32.0 °C |
12.0 Month @Temperature 41.0 - 89.6 °F |
|
3M Scotchkote™ 2400 Pipe Renewal Liner 3M Scotchkote Pipe Renewal Liner 2400 has been specifically developed for the rehabilitation of potable water pipe infrastructure to help extend service life, reduce leaks, and improve water quality.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | 10-25°C |
Amity Thermosets ATS 157 Phenolic Molding Long glass fiber Filler, Compression Molded Characteristics:Shock resistant ( High impact strength )Very good mechanical strengthGood dielectric strengthLow water absorptionLow shrinkageColor-pale brown, black, dark brown, green etc.Medium/st.. |
|||
Shelf Life | 12.0 Month @Temperature 23.0 °C |
12.0 Month @Temperature 73.4 °F |
|
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h.. |
|||
Shelf Life | 12.0 Month @Temperature 23.0 °C |
12.0 Month @Temperature 73.4 °F |
|
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
3M 200 Paper Tape 3M™ Paper Tape 200 is a utility purpose paper tape for holding, bundling, sealing, non-critical masking and a vast number of other jobs where a pressure-sensitive tape is needed.Information provide.. |
|||
Shelf Life | 12.0 Month @Temperature 23.9 °C |
12.0 Month @Temperature 75.0 °F |
|
Arlon R3781-920-##R##-P0 Silicone Rubber This fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicone tap.. |
|||
Shelf Life | 12.0 Month | 12.0 Month | |
Master Bond Supreme 46HT-2ND2 Two Component, Non-Drip, Toughened, Epoxy Adhesive Master Bond Polymer Supreme 46HT-2ND2 is a two component, non-drip, epoxy adhesive featuring an attractive balance of superior shear and peel strengths for high performance structural bonding suitab.. |