Processing Properties Metric English Comments
Dew Point -30.0 °C
-22.0 °F
Lubrizol Estane® GP 55 DB Thermoplastic Polyurethane
Type: Estane® GP 55DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding partsAvailable in EuropeInformation Provided by..
Dew Point -30.0 °C
-22.0 °F
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in..
Dew Point -30.0 °C
-22.0 °F
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Dew Point -30.0 °C
-22.0 °F
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Dew Point -30.0 °C
-22.0 °F
Lubrizol ESTANE® GP85AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 85AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Dew Point -30.0 °C
-22.0 °F
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane
Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E..