Processing Properties | Metric | English | Comments |
---|---|---|---|
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 4060D Sealant Grade PLA PLA (polylactide) polymer 4060D can be coextruded with other PLA resin to form a sealant layer for biaxially oriented PLA film. This resin has excellent heat seal and hot tack performance with a sea.. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6060D Fiber Grade PLA NatureWorks PLA polymer 6060D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6060D is designed for extrusion into mech.. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6201D Fiber Grade PLA NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically .. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6202D Fiber Grade PLA NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically .. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6204D Fiber Grade PLA NatureWorks® PLA polymer 6204D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6204D is designed for extrusion into mechanically .. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6251D Fiber Grade PLA NatureWorks® PLA polymer 6251D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6251D is designed for spunbond products using conv.. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6302D Fiber Grade PLA NatureWorks PLA polymer 6302D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6302D is designed for extrusion into mech.. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6751D Fiber Grade PLA NatureWorks® PLA polymer 6751D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6751D is designed for extrusion into mechanically .. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co.. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6350D Fiber Grade PLA NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into s.. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6400D Fiber Grade PLA NatureWorks® PLA polymer 6400D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6400D is designed for extrusion into mechanically .. |
|||
Dew Point | -35.0 °C | -31.0 °F | |
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f.. |