Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.0167 - 43200 min | 0.000278 - 720 hour | Average value: 492 min Grade Count:280 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Cure Time | 3.00 - 43200 min | 0.0500 - 720 hour | Average value: 4860 min Grade Count:57 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Cure Time | 10800 - 43200 min | 180 - 720 hour | |
Humiseal 1A27 Urethane Conformal Coating Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit.. |
|||
Cure Time | 10800 - 43200 min | 180 - 720 hour | |
Humiseal 1A27LSE Urethane Conformal Coating Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C).. |
|||
Cure Time | 10800 - 43200 min | 180 - 720 hour | |
Humiseal 1A33 Urethane Conformal Coating Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL.. |
|||
Cure Time | 10800 - 43200 min | 180 - 720 hour | |
Humiseal 1A33LSE Urethane Conformal Coating Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther.. |