Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | <= 1.00 min | <= 0.0167 hour | With Primer (Fixture) |
ND Industries NutGrade® 122 Removable Threadlocker A medium strength, oil tolerant threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or b.. |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | handling time |
Permabond TA436 Toughened Acrylic Adhesive PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength.. |
|||
Cure Time | <= 1.00 min | <= 0.0167 hour | Polycarbonate, fixture time, (low power 4mW lamp) |
Permabond UV648 UV-curable Adhesive PERMABOND UV648 is a UV-curing adhesive developed for use on plastics. It has good adhesion to acrylic and contains a long-wavelength photo initiator to allow it to cure through UV-stabilized plasti.. |
|||
Cure Time | 1.00 - 3.00 min @Temperature 204 - 260 °C |
0.0167 - 0.0500 hour @Temperature 399 - 500 °F |
|
Lord Adhesives Flocklok® 550P Flock Adhesive LORD Flocklok® 550P adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of uncured and semi-cured elastomers including EPDM, NR, CR and SBR. Flocked sub.. |
|||
Cure Time | 1.00 min | 0.0167 hour | Fixture time |
ITW Devcon One minuteâ„¢ Epoxy Gel, Amber Information provided by ITW Devcon |
|||
Cure Time | 1.00 - 3.00 min @Temperature 140 - 160 °C |
0.0167 - 0.0500 hour @Temperature 284 - 320 °F |
|
Lucite International Colacryl ® TS1631 Acrylic Solution Resin Acrylic copolymer with reactive groupsA highly flexible resin with good handle. It exhibits good adhesion, resistance to ageing and light stability.Suggested Use: Coating and lamination of nylon and.. |
|||
Cure Time | 1.00 min | 0.0167 hour | At 30 mW/cm2 |
Tra-Con Tra-Bond 546S02 Low Viscosity UV Curable Adhesive TRA-BOND 546S02 is a low viscosity UV curable adhesive exhibiting exceptional adhesion to glass. TRA-BOND 546S02 is designed to be semi-flexible resulting in stress free bonds to glass and other sub.. |
|||
Cure Time | 1.00 min | 0.0167 hour | UV Full Cure in 60 seconds at 75 mW/cm^2 |
Loctite® 5072 Silicone Chip Coating Conformal CoatingsConformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Locti.. |
|||
Cure Time | 1.00 min | 0.0167 hour | Dry Time |
Loctite® 7113 Heptane Base Accelerator Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |
|||
Cure Time | 1.00 min | 0.0167 hour | |
Loctite® SpeedBonder™ 326 Fast Fixture Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Cure Time | 1.00 min @Temperature 150 °C |
0.0167 hour @Temperature 302 °F |
|
Dow Corning SR-7010 Two-part, hard, clear LED resin with a high refractive index and excellent light transparency, for molding fabricated parts.Information provided by Dow Corning |
|||
Cure Time | 1.00 - 6.00 min | 0.0167 - 0.100 hour | ts2; ASTM D2084 |
ExxonMobil Exxon™ 2244 Fast Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber bales.Information provided by ExxonMobil Chemical |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-30 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-31 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-32 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-33 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-34 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-37 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 10.0 min | 0.0167 - 0.167 hour | |
Abatron L060330-2 Flexible Polyurea Compound L060330-2 is used for castings, repairs, assemblies, coatings, and laminations that require fast hardening. It is also used for bonding most rigid materials such as metals, aluminum, copper, china, .. |
|||
Cure Time | 1.00 - 2.00 min | 0.0167 - 0.0333 hour | |
3M Scotch-Weld™ CA50 Gel Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. High-viscosity, non-sag gel and less sensitive to acidic surfaces.Information provided by 3M |
|||
Cure Time | 1.00 min | 0.0167 hour | Set Time |
3M Scotch-Weld™ EZ250060 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Cure Time | 1.00 min | 0.0167 hour | Set Time |
3M Scotch-Weld™ TE100 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Cure Time | 1.00 min | 0.0167 hour | Set Time |
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Cure Time | 1.00 min | 0.0167 hour | Tack-free |
3M FIP 1-Step Fire Barrier Rated Foam 3M Fire Barrier Rated Foam (FIP 1-Step), is a smoke, sound, and firestopping foam for wall and floor penetrations. Premium two-part, easy-to-handle formulations. Expands up to five times during inst.. |
|||
Cure Time | 1.00 - 1.50 min @Temperature 150 °C |
0.0167 - 0.0250 hour @Temperature 302 °F |
|
Loctite® CHIPBONDER® 3615 High Adhesion, Syringe Dispense Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te.. |
|||
Cure Time | 1.00 - 1.50 min @Temperature 150 °C |
0.0167 - 0.0250 hour @Temperature 302 °F |
|
Loctite® CHIPBONDER® 3618 High Speed, Syringe Dispense Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te.. |
|||
Cure Time | 1.00 min | 0.0167 hour | at 40 mW/cm^2 |
Loctite® Nuva-Sil® 5088 Potting Compound Potters and Silicon Light Cure AdhesivesLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and sho.. |
|||
Cure Time | 1.00 min | 0.0167 hour | at 70 mW/cm^2 |
Loctite® Nuva-Sil® 5092 Non-corrosive Potting Silicon Light Cure Adhesives and PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and sho.. |