Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 4.00 - 6.00 min
0.0667 - 0.100 hour
handling time
Permabond ET500 Epoxy Resin
PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera..
Cure Time 4.02 - 6.00 min
0.0670 - 0.100 hour
working strength
Permabond TA4810 Toughened Acrylic Adhesive
PERMABOND TA4810 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites.  TA4810 has excellent adhesion to as received metal surfac..
Cure Time 3.00 - 6.00 min
0.0500 - 0.100 hour
Working time
ITW Devcon 5 minute® Epoxy, Light Amber
Information provided by ITW Devcon
Cure Time 4.00 - 6.00 min
0.0667 - 0.100 hour
Working time
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive SD, Off-White
Information provided by ITW Devcon
Cure Time 4.00 - 6.00 min
0.0667 - 0.100 hour
Working time
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive, Straw, White, Black
Information provided by ITW Devcon
Cure Time 1.00 - 6.00 min
0.0167 - 0.100 hour
ts2; ASTM D2084
ExxonMobil Exxon™ 2244 Fast Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber bales.Information provided by ExxonMobil Chemical