Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JLX2 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability Information provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 Description: UBESTA has a strong resistance to chemicalsInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethylacetate for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hexane for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Toluene for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Water for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Screw Speed | 15 - 76 rpm | 15 - 76 rpm | For 8x1 mm Tube Extrusion |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |