Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Screw Speed = 15 rpm Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3020X8 Nylon 12 Thermister
Description: UBESTA Nylon 12 ThermisterInformation provided by UBE.
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3024LU Rigid Black Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE.
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JI9L 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability, designed for high burst pressure performance at high temperat..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE.
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE.
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Ethanol for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Ethanol for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12
Description: UBESTA has a strong resistance to chemicalsInformation provided by UBE.
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Fuel C/E10 for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Methanol for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Trichloroethylene for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030XA Nylon 12 Film
Description: UBESTA Nylon 12 FilmInformation provided by UBE.
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12
Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron..
Screw Speed 15 - 70 rpm
15 - 70 rpm
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane
Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and ..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Methanol for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Xylene for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..