Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N2033STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N2043HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N2043L Nylon 6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (Cond) Information provided by Ravago |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B.. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1040MGL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax PBT 3030-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | |
LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified 13% glass-filled impact modified nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax PBT 2000-201D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax PBT 3030-104 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-2028A UMB Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-2678C Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-7010-73NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-7100-87 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® GFT13-66 XE-N 13% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® GS40-60 42LH-N 40% Glass Sphere Filled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® MRGF30/10 42H-N 30% Mineral/10% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® T-731E-BK 10% Reinforced Abrasion Resistant Nylon 6 Description: Abrasion Resistant Nylon 6Information provided by Wellman. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® 7010-73NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-7010-55NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | |
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax PBT 4115-201D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |