Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact Polycarbonate, General Purpose, Low FlowFeatures: • Food Contact AcceptableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
DuPont Performance Polymers Crastin® LW9320 BK851 PBT
(Unverified Data**) Crastin® LW9320 BK851 is a 20% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET
(Unverified Data**) Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
DuPont Performance Polymers Delrin® 127UVE RD402 Acetal Homopolymer
(Unverified Data**) Delrin® 127UVE RD402 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Pasargad Polymer Peyvand Pasamid 3P-H1150B Nylon 6, 50% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
DuPont Performance Polymers Zytel® 101L BKB009 Nylon 66
(Unverified Data**) Zytel® 101L BKB009 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
DuPont Performance Polymers Zytel® 70G35EF NC010 Nylon 66
(Unverified Data**) Zytel® 70G35EF NC010 is a 35% glass reinforced polyamide 66 developed for electrical and electronics applications.Information provided by DuPont Performance Polymers |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM; Dehumidified Dryer; Injection Molding |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
LG Chemical KEYFLEX BT 1030D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
LG Chemical KEYFLEX TO1065A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
LG Chemical LUPOL HI5204G PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
DuPont Performance Polymers Zytel® EFE8089B BK416 Nylon 66 Zytel® EFE8089B BK416 is a 33% fiber reinforced, heat stabilized, lubricated, toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET
(Unverified Data**) Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Handling |
Aremco Corr-Paint™ CP4040-S High Temperature Protective Coating Silicone-Polyester |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Lubrizol Estane® 58437 Thermoplastic Polyurethane Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi.. |