Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Dry Time | 2.50 - 4.00 hour | 2.50 - 4.00 hour | |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil.. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil.. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st.. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st.. |
|||
Dry Time | 2.50 - 3.50 hour | 2.50 - 3.50 hour | |
Solvay Specialty Polymers Udel® M-2300 MR Polysulfone (PSU), Mold Release
(discontinued **) Udel M-2300 MR is an injection-moldable, low-color grade of polysulfone that is nearly water white in color. This material contains a mold release which aids part ejection when parts with low draft .. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta.. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta.. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and .. |
|||
Dry Time | 2.50 - 4.00 hour | 2.50 - 4.00 hour | |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to .. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Dry Time | 2.50 - 4.00 hour | 2.50 - 4.00 hour | |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Dry Time | 2.50 - 4.00 hour | 2.50 - 4.00 hour | |
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Dry Time | 2.50 hour | 2.50 hour | |
Solvay Specialty Polymers Veradel® 3300 Polyethersulfone (PESU)
(discontinued **) Veradel 3300 polyethersulfone (PESU) is a medium melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, b.. |