Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 149 - 175 °C | 300 - 347 °F | Average value: 151 °C Grade Count:7 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Drying Temperature | 150 - 175 °C | 302 - 347 °F | |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Drying Temperature | 150 - 175 °C @Time 9000 - 14400 sec |
302 - 347 °F @Time 2.50 - 4.00 hour |
|
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |