Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 70.0 - 75.0 °C @Time 14400 sec |
158 - 167 °F @Time 4.00 hour |
|
Chi Mei Acryrex® CM-211 PMMA Features:Good Weather ResistanceHigh ClarityHigh FlowHigh GlossHigh Heat ResistanceHigh ViscosityUses:ContainersCosmeticsHousehold GoodsKnobsRoHS CompliantAppearance: Clear/TransparentForms: Pellets.. |
|||
Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
Arkema Group Pebax® 5533 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
Arkema Group Pebax® 5533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
Arkema Group Pebax® 5533 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
Arkema Group Pebax® 6333 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
Arkema Group Pebax® Rnew 55R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 55R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |