Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Drying Temperature | 100 °C | 212 °F | |
Plastcom SLOVASTER® B1 GF 20 000/2 PBT, 20% glass fibre FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre, excellent flow. Characterised by excellent properties also at minus temperatures like eg. modu.. |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | |
Polykemi AB POLYblend 45FS GKF2010 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | |
Polykemi AB POLYblend 85FS UV PC/ABS-Blend, UV stabilized Information provided by Polykemi AB |
|||
Drying Temperature | 100 - 121 °C | 212 - 250 °F | Average value: 119 °C Grade Count:14 |
Overview of materials for Polyarylamide, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | Injection Molding |
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY GP1000MU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY GP1006FM PC, Flame Retardant Description: Injection Molding, PC, Flame RetardantApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U.. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 100 °C | 212 °F | |
Unitika AX-1500 Conditioned AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Drying Temperature | 100 °C | 212 °F | |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Drying Temperature | 100 °C | 212 °F | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 100 °C | 212 °F | |
Unitika UM-8400-20 Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Drying Temperature | 100 °C | 212 °F | |
BASF Ultraform® S2320 003 PRO POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
Asia International Enterprise (Hong Kong) 3010FW Polybutylene terephthalate Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | Requested for non-reinforced self-extinguishing types. Temperature can be reduced when using vacuum ovens. |
LATI LARIL 13 Light Brown Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |