Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ABS/PC 7901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ABS/PC 9901 Description: Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA S310 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA S319 Description: ASA Weatherable Polymer, Injection Molding Grade, High ModulusInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA S519 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA S610 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA S710 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA T-120 Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA TW-17 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA TW-18B2 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA TW-20 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA TW-23V Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA/PC TA-35 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ABS/PC 8901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
Diamond Polymers ABS/PC 9801 Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc. |