Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
LTL Color Compounds ColorFast® FRA203 ABS Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® OBC 4665A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® OBC 4873A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL EF-6133L2 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL EF-6162 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1182A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1183A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1295B Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Soft Touch Applications; Flexible Grips; Handles; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: M.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1472A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-150 BLK288 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1522E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1522H Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1536D Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Household Goods; Food Containers; Handles; Lids Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2460B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2478H Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2565F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2590F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2597 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2635A Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2635D Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-3260R Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-6085 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-81-D965-P Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-83-F912-ER Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-86-K875-F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1996E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-86-K986-A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-97-T0214B-55 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |