Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Rear Barrel Temperature = 331 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE)
Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora..
Rear Barrel Temperature 166 - 182 °C
331 - 360 °F
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds..
Rear Barrel Temperature 166 - 182 °C
331 - 360 °F
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 ..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE)
The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro..
Rear Barrel Temperature 166 - 193 °C
331 - 379 °F
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
Rear Barrel Temperature 166 - 193 °C
331 - 379 °F
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE)
Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established...
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G2755C Thermoplastic Elastomer (TPE)
Dynaflex™ G2755C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypropylene ..
Rear Barrel Temperature 166 - 204 °C
331 - 399 °F
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - ..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7940-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7940-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7940-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7940-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7960-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Dynaflex™ G7980-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Dynaflex™ G7980-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Dynaflex™ G7990-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7990-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-1001-00 can be re..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Dynaflex™ G7990-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7990-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-9001-02 can be re..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7690-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7690-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Rear Barrel Temperature 166 - 182 °C
331 - 360 °F
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE)
Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Rear Barrel Temperature 166 - 177 °C
331 - 351 °F
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl..
Copyright © lookpolymers.com All Rights Reserved