Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Dynaflex™ G2755C Thermoplastic Elastomer (TPE) Dynaflex™ G2755C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypropylene .. |
|||
Rear Barrel Temperature | 149 - 177 °C | 300 - 351 °F | |
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Rear Barrel Temperature | 160 - 177 °C | 320 - 351 °F | |
PolyOne Dynaflex™ G7930-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Dynaflex™ G7940-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Rear Barrel Temperature | 160 - 177 °C | 320 - 351 °F | |
PolyOne Dynaflex™ G7950-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Rear Barrel Temperature | 160 - 177 °C | 320 - 351 °F | |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Rear Barrel Temperature | 160 - 177 °C | 320 - 351 °F | |
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Dynaflex™ G7960-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Rear Barrel Temperature | 154 - 177 °C | 309 - 351 °F | |
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol.. |
|||
Rear Barrel Temperature | 149 - 177 °C | 300 - 351 °F | |
PolyOne Dynaflex™ G6713C Thermoplastic Elastomer (TPE) Dynaflex™ G6713C is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV Sta.. |
|||
Rear Barrel Temperature | 160 - 177 °C | 320 - 351 °F | |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Dynaflex™ G7690-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Dynaflex™ G7960-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Green Dot Terratek® BD 4015 Biodegradable Polymer Terratek BD biodegradable composites are created from a proprietary blend of starch-based ingredients and other materials, the natural components derived from renewable grain sources account for the.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® 2840 Thermoplastic Elastomer Elastocon® 2840 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2840 is FDA compliant and well suited for cons.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer Elastocon® 2850PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2850PE is FDA compliant and well suited for.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® 2860L Thermoplastic Elastomer Elastocon® 2860L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2860L is FDA compliant and well s.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® 2870 Thermoplastic Elastomer Elastocon® 2870 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2870 is FDA compliant and well suited for cons.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® 2880L Thermoplastic Elastomer Elastocon® 2880L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2880L is FDA compliant and well s.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® 8068B Thermoplastic Elastomer Elastocon® 8068B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068B is well suited for consumer goods an.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® 8068N Thermoplastic Elastomer Elastocon® 8068N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068N is FDA compliant and well suited.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® CLR45 Thermoplastic Elastomer Elastocon® CLR45 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR45 is.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® CLR65 Thermoplastic Elastomer Elastocon® CLR65 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a tactile surface finish. Elastoc.. |
|||
Rear Barrel Temperature | 166 - 177 °C | 330 - 350 °F | |
Elastocon TPE Technologies Elastocon® OF75 Thermoplastic Elastomer Elastocon® OF75 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a reduced coefficient of friction. Ela.. |