Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well suited for consumer goods and industrial applications requiring increased U.V. stability. Elastocon® 8068BL can be overmolded to polypropylene.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.021 cm/cm
0.0010 - 0.021 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
ASTM D2240
Tensile Strength, Yield 7.93 MPa
1150 psi
ASTM D412
Elongation at Break 660 %
660 %
ASTM D412
100% Modulus 0.00296 GPa
0.430 ksi
ASTM D412
Compression Set 20 %

@Time 79200 sec
20 %

@Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Feed Temperature 79.0 °C
174 °F
Rear Barrel Temperature 166 - 177 °C
330 - 350 °F
Front Barrel Temperature 177 - 182 °C
350 - 360 °F
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Descriptive Properties Value Comments
Injection Rate Fast