Polymer Property : Mold Temperature = 150 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 4.44 - 65.6 °C
40.0 - 150 °F
Multibase Multi-Pro® 3014 XUGW Polypropylene
Mineral Filled.Features:Gloss, HighUV Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Multibase
Mold Temperature 10.0 - 65.6 °C
50.0 - 150 °F
Injection Molding
Teknor Apex Sarlink® 3190 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3190 can be processed by blow molding, injection molding or..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-1081B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-1140D BLK Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Interior Parts; Blow Molding Applications; Carpet Backing; General Purpose; Grommets; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injectio..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-2585F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-83-F912-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-86-K875-F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Teknor Apex Telcar® TL-86-K902A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Mold Temperature 30.0 - 65.6 °C
86.0 - 150 °F
A. Schulman SCHULADUR® A GB20 20% Glass Bead Reinforced PBT
Information provided by A. Schulman.
Mold Temperature 10.0 - 65.6 °C
50.0 - 150 °F
Average value: 44.2 °C Grade Count:35
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..