Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 35.0 - 121 °C | 95.0 - 250 °F | Average value: 93.9 °C Grade Count:100 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Mold Temperature | 35.0 - 121 °C | 95.0 - 250 °F | Average value: 95.7 °C Grade Count:53 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Mold Temperature | 35.0 °C | 95.0 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T85UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T85UV is a UV resistant polycaprolactone copolyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, featuring adequate hardness with excellent.. |
|||
Mold Temperature | 35.0 °C | 95.0 °F | |
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colou.. |
|||
Mold Temperature | 35.0 °C | 95.0 °F | |
Multibase Multi-Flex® TEA 4001-35 Natural TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP 1061 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1320E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1488A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1564-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1578 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1580B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1644L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1698 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1890UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2132 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2215 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2285CMT Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2290 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2295 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2327R1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP 1128 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP 1225B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP 1227A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1357A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1389E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2455S Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2579A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2790 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 °C | 95.0 °F | |
Borealis BorPURE™ RE450MO Polypropylene Random Copolymer BorPure™ RE450MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is characterized by optimum combination of high impact strength and.. |
|||
Mold Temperature | 35.0 °C | 95.0 °F | Injection Molding |
Covestro Texin® 990 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer Mater.. |