Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products GC10P250-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural Applications: Component housingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products M25P251-01A 25% Mica Reinforced Polypropylene Copolymer, Black Applications: Fan shroudsInternal I/P componentsFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products P256-01A Polypropylene Copolymer, Black Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products T20P250-01 20% Talc Reinforced Polypropylene Copolymer, Black Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products T30P200-01BG 30% Talc Reinforced Polypropylene Copolymer, Black, Blow Molding Grade Applications: HVAC ductsSeat backsFlipper panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products F15-00UV 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV-Stabilized, Natural Applications: Functional SupportsElectrical housingsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products HP531-678UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, IT3A Medium Light Stone Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 15.6 - 48.9 °C | 60.0 - 120 °F | |
Green Dot Terratek® BD 4015 Biodegradable Polymer Terratek BD biodegradable composites are created from a proprietary blend of starch-based ingredients and other materials, the natural components derived from renewable grain sources account for the.. |
|||
Mold Temperature | 37.8 - 48.9 °C | 100 - 120 °F | |
Star Plastics ABS3030 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 37.8 - 48.9 °C | 100 - 120 °F | |
Star Plastics ABSHFL Molding Grade ABS High Flow Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP 1079E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1473F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1580L1-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1646-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1662-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1791R4 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1907E CLR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2295 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-1855PV2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2564B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2775 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2820M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2830E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP-2850M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Mold Temperature | 15.6 - 48.9 °C | 60.0 - 120 °F | |
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and .. |
|||
Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
Teknor Apex Monprene® MP 1245A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |