Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 180 - 230 °C | 356 - 446 °F | |
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ CLS 5000 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ FFSL 7061 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LIM 6030 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2010 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2030 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2080 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2560 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2610 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2620 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2641 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2680FC High Productivity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2725/40 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2735/30 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2740 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2742 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2752 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2841 Liquid Silicone Rubber - Good Flex Life This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/60 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3596/30 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3696/20 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4020 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 7080 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT HE Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating - Physical Properties are subject to the substrate that is used. |
|||
Mold Temperature | 180 - 230 °C | 356 - 446 °F | |
Lehmann & Voss LUVOCOM® 1104-7598 Polyether ketone, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str.. |
|||
Mold Temperature | 160 - 230 °C | 320 - 446 °F | |
Lehmann & Voss LUVOCOM® 1114-0717 PAEK, with carbon fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/70 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Silopren™ LSR 3386/30 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |